PET GF20 with 20% Glass Fiber Reinforcement – Nylon Plastic

PET GF20 is an engineering thermoplastic based on Polyethylene Terephthalate (PET) reinforced with 20% glass fibers. This versatile grade strikes an ideal balance between enhanced mechanical performance, superior dimensional precision, and good aesthetics, making it a preferred choice for high-quality technical parts across various industries.

Why Choose Our PET GF20?
✅ Master of Balance for Technical Parts: We supply a material that excels in providing a harmonious combination of strength, precision, and surface quality, enabling the production of reliable and visually acceptable engineering components.
✅ Engineered for Predictable Performance: Our PET GF20 is formulated for consistent processing and stable performance, giving you confidence in part consistency and long-term reliability.
✅ Dedicated Support for Complex Designs: We offer the technical expertise to help you optimize tool design and processing parameters for PET GF20, ensuring success even with intricate part geometries.
✅ Enabling Innovation in Demanding Sectors: We help you leverage this balanced material in automotive, electronics, and consumer durables where both technical performance and part quality are critical.

Category: Brand:

万翰详情 01

PET GF20 Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 20% ISO 1172
Tensile Strength 125 – 145 MPa ISO 527
Flexural Modulus 8,500 – 10,000 MPa ISO 178
Notched Impact Strength 7 – 9 kJ/m² ISO 180
HDT @1.8 MPa 215 – 225 °C ISO 75
Comparative Tracking Index (CTI) 575 V IEC 60112

PET GF Series Performance Comparison Table (Estimated Typical Values)

Property PET GF10 PET GF20 PET GF30 PET GF40 PET GF50
Glass Fiber Content 10% 20% 30% 40% 50%
Tensile Strength 100 – 120 MPa 125 – 145 MPa 145 – 165 MPa 160 – 180 MPa 175 – 195 MPa
Flexural Modulus 7,000 – 8,500 MPa 8,500 – 10,000 MPa 10,000 – 12,000 MPa 12,000 – 14,000 MPa 14,000 – 17,000 MPa
Notched Impact Strength 6 – 8 kJ/m² 7 – 9 kJ/m² 8 – 11 kJ/m² 7 – 10 kJ/m² 6 – 9 kJ/m²
HDT @1.8 MPa 205 – 215 °C 215 – 225 °C 225 – 235 °C 230 – 240 °C 235 – 245 °C
CTI (Comparative Tracking Index) 600 V 575 V 550 V 525 V 500 V
Key Profile Cost-effective high-strength upgrade Precision parts with great surface Best all-around structural performance High rigidity & creep resistance Maximum stiffness for metal replacemen

PET GF20 Key Advantages

✅ Enhanced Stiffness & Surface Finish: Delivers a notable increase in rigidity and strength over GF10 while maintaining the capacity for a very good surface finish, which is often a challenge with higher fiber content.
✅ Precision Engineering Grade: Offers an excellent balance of high mechanical properties, predictable low shrinkage, and good dimensional stability for molding complex, tight-tolerance components.
✅ Robust Performance in Demanding Environments: Provides improved thermal capabilities and maintains good chemical resistance, suitable for more demanding mechanical and electrical applications.

Industry Applications:

the crucial role of injection molding in automotive industry

Explore the PET Glass Fiber Series in Detail

Click on the links below to view comprehensive technical data, key advantages, and application details for each specific grade.

Grade Best For Overview Full Details
PET GF10 Cost-effective upgrade for high-strength, dimensionally stable parts. The most accessible GF grade, offering a significant boost in strength, stiffness, and heat resistance over unfilled PET. View PET GF10 Full Data Sheet →
PET GF20 Precision components requiring an excellent surface finish and high mechanical properties. A balanced performer with superior dimensional stability, good processability, and high surface quality for engineering parts. View PET GF20 Full Data Sheet →
PET GF30 High-performance structural parts under significant thermal and mechanical stress. The industry benchmark grade, delivering an optimal balance of very high strength, rigidity, heat resistance, and stability. View PET GF30 Full Data Sheet →
PET GF40 Ultra-stiff, high-load applications where minimal creep and deflection are critical. Engineered for maximum rigidity and exceptional long-term dimensional stability under continuous load at high temperatures. View PET GF40 Full Data Sheet →
PET GF50 Maximum mechanical performance for demanding metal replacement applications. The pinnacle grade, offering the highest stiffness, strength, and thermal resistance in the series for the most challenging applications. View PET GF50 Full Data Sheet →

Powering Innovation Across Industries

Industry Key Applications
Automotive High-temperature under-the-hood components (sensor housings, connectors, coil bobbins), structural brackets, lamp sockets and reflectors, wiper system parts. Explore Automotive Applications →
Electrical & Electronics Miniaturized and high-pin-count connectors, circuit breakers, switch housings, motor components (commutators, end caps), transformer bobbins. Discover E&E Solutions →
Industrial Equipment High-load gears, bearings, pump housings and impellers, conveyor system components, robotic structural parts requiring stiffness and creep resistance. See Industrial Uses →
Consumer Goods & Appliances Power tool housings and gears, kitchen appliance components (hand mixer housings, blender bases), high-strength consumer electronics housings. Explore Consumer Applications →
Packaging & Technical Parts Reusable industrial containers (totes, pallets), thin-walled but rigid technical packaging, components requiring inherent gas barrier properties. Inquire About Special Uses →

Various application scenarios of PA plastics

Various application scenarios of PA plastics

 How to Choose the Right PET GF Grade?

In simple terms:
For a cost-effective performance upgrade with significantly enhanced strength, stiffness, and heat resistance for structural parts, consider PET GF10.
For the optimal balance of high mechanical properties, excellent surface finish, and dimensional precision in demanding technical components, choose PET GF30. It is the performance benchmark for most structural applications.
For the ultimate stiffness, strength, and long-term dimensional stability under extreme load and heat, consider PET GF50.
Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation: https://nylonplastic.com/contact/

Why Choose Us?

万翰详情 03

万翰详情 04

PET GF20 FAQ
Q1: When should I choose PET GF20 over GF10?
Choose PET GF20 when your application requires higher mechanical strength, greater rigidity, and better thermal resistance than GF10 can provide, and where excellent dimensional stability and good surface finish are also important. It is ideal for more structurally demanding yet appearance-sensitive parts.

Q2: Can PET GF20 be used for gears or bearings?
Yes, it is a strong candidate. Its combination of high stiffness, low friction, good wear resistance, and excellent dimensional stability makes PET GF20 suitable for light-to-moderate duty gears, bearings, and bushings, especially where exposure to moderate heat is a factor.

Q3: How does its processability compare to PET GF30?
PET GF20 generally has better flow and easier processing than GF30 due to its lower fiber content. It can fill thinner walls and complex molds more readily and typically exhibits less wear on tooling. It offers a good compromise between performance and ease of manufacturing.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information