PET GF30 with 30% Glass Fiber Reinforcement – Nylon Plastic

PET GF30 is an engineering thermoplastic based on Polyethylene Terephthalate (PET) reinforced with 30% glass fibers. This high-performance grade is the industry benchmark, engineered to deliver an unmatched combination of mechanical strength, thermal resilience, and dimensional stability for the most demanding structural and electrical applications.

Why Choose Our PET GF30?
✅ The Gold Standard for Structural Polyesters: We supply the definitive PET grade where peak performance is required, ensuring reliability in automotive, electrical, and mechanical systems.
✅ Engineered for Precision Under Pressure: Our PET GF30 guarantees that critical components maintain their geometry and strength under continuous stress and high-temperature environments.
✅ Expert Support for Demanding Processing: We provide specialized guidance on drying and molding crystalline PET to help you achieve optimal mechanical properties and surface quality.
✅ Driving Innovation in High-Tech Sectors: We enable advancements in applications ranging from automotive engine compartments to electrical enclosures by providing a material that exceeds rigorous performance expectations.

Category: Brand:

万翰详情 01

PET GF30 Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 30% ISO 1172
Tensile Strength 145 – 165 MPa ISO 527
Flexural Modulus 10,000 – 12,000 MPa ISO 178
Notched Impact Strength 8 – 11 kJ/m² ISO 180
HDT @1.8 MPa 225 – 235 °C ISO 75
Comparative Tracking Index (CTI) 550 V IEC 60112

PET GF Series Performance Comparison Table (Estimated Typical Values)

Property PET GF10 PET GF20 PET GF30 PET GF40 PET GF50
Glass Fiber Content 10% 20% 30% 40% 50%
Tensile Strength 100 – 120 MPa 125 – 145 MPa 145 – 165 MPa 160 – 180 MPa 175 – 195 MPa
Flexural Modulus 7,000 – 8,500 MPa 8,500 – 10,000 MPa 10,000 – 12,000 MPa 12,000 – 14,000 MPa 14,000 – 17,000 MPa
Notched Impact Strength 6 – 8 kJ/m² 7 – 9 kJ/m² 8 – 11 kJ/m² 7 – 10 kJ/m² 6 – 9 kJ/m²
HDT @1.8 MPa 205 – 215 °C 215 – 225 °C 225 – 235 °C 230 – 240 °C 235 – 245 °C
CTI (Comparative Tracking Index) 600 V 575 V 550 V 525 V 500 V
Key Profile Cost-effective high-strength upgrade Precision parts with great surface Best all-around structural performance High rigidity & creep resistance Maximum stiffness for metal replacemen

PET GF30 Key Advantages

✅ Benchmark High-Strength Performance: Offers an exceptional balance of very high tensile strength, rigidity, and impact resistance, setting the standard for structural polyester components.
✅ Superior Heat Resistance & Dimensional Stability: Features one of the highest heat deflection temperatures among common engineering thermoplastics, coupled with extremely low moisture absorption and shrinkage for precision parts.
✅ Excellent Electrical Insulation & Creep Resistance: Maintains good dielectric properties while providing outstanding resistance to deformation under long-term load, even at elevated temperatures.

Industry Applications:

the crucial role of injection molding in automotive industry

Explore the PET Glass Fiber Series in Detail

Click on the links below to view comprehensive technical data, key advantages, and application details for each specific grade.

Grade Best For Overview Full Details
PET GF10 Cost-effective upgrade for high-strength, dimensionally stable parts. The most accessible GF grade, offering a significant boost in strength, stiffness, and heat resistance over unfilled PET. View PET GF10 Full Data Sheet →
PET GF20 Precision components requiring an excellent surface finish and high mechanical properties. A balanced performer with superior dimensional stability, good processability, and high surface quality for engineering parts. View PET GF20 Full Data Sheet →
PET GF30 High-performance structural parts under significant thermal and mechanical stress. The industry benchmark grade, delivering an optimal balance of very high strength, rigidity, heat resistance, and stability. View PET GF30 Full Data Sheet →
PET GF40 Ultra-stiff, high-load applications where minimal creep and deflection are critical. Engineered for maximum rigidity and exceptional long-term dimensional stability under continuous load at high temperatures. View PET GF40 Full Data Sheet →
PET GF50 Maximum mechanical performance for demanding metal replacement applications. The pinnacle grade, offering the highest stiffness, strength, and thermal resistance in the series for the most challenging applications. View PET GF50 Full Data Sheet →

Powering Innovation Across Industries

Industry Key Applications
Automotive High-temperature under-the-hood components (sensor housings, connectors, coil bobbins), structural brackets, lamp sockets and reflectors, wiper system parts. Explore Automotive Applications →
Electrical & Electronics Miniaturized and high-pin-count connectors, circuit breakers, switch housings, motor components (commutators, end caps), transformer bobbins. Discover E&E Solutions →
Industrial Equipment High-load gears, bearings, pump housings and impellers, conveyor system components, robotic structural parts requiring stiffness and creep resistance. See Industrial Uses →
Consumer Goods & Appliances Power tool housings and gears, kitchen appliance components (hand mixer housings, blender bases), high-strength consumer electronics housings. Explore Consumer Applications →
Packaging & Technical Parts Reusable industrial containers (totes, pallets), thin-walled but rigid technical packaging, components requiring inherent gas barrier properties. Inquire About Special Uses →

Various application scenarios of PA plastics

 How to Choose the Right PET GF Grade?

In simple terms:
For a cost-effective performance upgrade with significantly enhanced strength, stiffness, and heat resistance for structural parts, consider PET GF10.
For the optimal balance of high mechanical properties, excellent surface finish, and dimensional precision in demanding technical components, choose PET GF30. It is the performance benchmark for most structural applications.
For the ultimate stiffness, strength, and long-term dimensional stability under extreme load and heat, consider PET GF50.
Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation: https://nylonplastic.com/contact/

Why Choose Us?

万翰详情 03

万翰详情 04

PET GF30 FAQ
Q1: What are the main differences between PET GF and PBT GF?
PET GF typically offers higher tensile strength, higher heat deflection temperature (by ~20-30°C), and better gas barrier properties than PBT GF of the same fiber content. However, PET is more sensitive to hydrolysis during processing (requires more thorough drying) and can have a narrower processing window. PBT generally offers faster cycle times and better surface finish.

Q2: Is PET GF30 suitable for under-the-hood automotive parts?
Yes, it is an excellent candidate. Its high HDT (over 220°C), good mechanical properties retention at high temperatures, and resistance to oils and coolants make it suitable for components like sensor housings, connectors, and structural brackets in the engine compartment.

Q3: What is the most critical step in processing PET GF30?
Thorough drying is absolutely critical. PET is highly susceptible to hydrolysis (molecular degradation by moisture) at melt temperatures. Material must be dried to below 0.02% moisture content, typically at 120-140°C for 4-6 hours in a dehumidifying dryer. Improper drying leads to severe loss of mechanical properties.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information