PC/ABS GF20 with 20% Glass Fiber Reinforcement – Nylon Plastic

PC/ABS Reinforced (GF20) is an advanced engineering composite based on the PC/ABS alloy matrix reinforced with 20% glass fibers. This grade is engineered for applications where the base alloy‘s properties are insufficient, specifically targeting requirements for exceptional rigidity, dimensional precision under thermal and mechanical stress, and enhanced long-term performance.

Why Choose Our PC/ABS Reinforced (GF20)?
✅ Polymer Solution for High Stiffness: When your design needs metal-like rigidity but desires the design freedom and lightweight of plastics, GF20 is the perfect answer.
✅ Ensures Dimensional Permanence for Precision Parts: Our material offers exceptional dimensional stability, ideal for precision gears, bearing housings, brackets, and parts with tight assembly tolerances.
✅ Tackles Structural Challenges in Hot Environments: Its improved HDT and creep resistance make it suitable for parts near automotive engine bays or inside high-speed electrical devices.
✅ Expert Support for Reinforced Materials Processing: We provide specialized guidance on equipment and process requirements (e.g., wear-resistant screws/tooling) for smooth production startup.

Category: Brand:

万翰详情 01

 

PC/ABS Reinforced (GF20) Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 20% ISO 1172
Tensile Strength 70 – 85 MPa ISO 527
Flexural Modulus 4,500 – 5,500 MPa ISO 178
Notched Impact Strength 15 – 25 kJ/m² ISO 180
HDT @1.8 MPa 115 – 125 °C ISO 75
Mold Shrinkage 0.2 – 0.4% ISO 294-4

PC/ABS Series Performance Comparison Table (Estimated Typical Values)

Property PC/ABS GP PC/ABS HF PC/ABS FR (V-0) PC/ABS GF20
Tensile Strength 50 – 60 MPa 48 – 55 MPa 45 – 55 MPa 70 – 85 MPa
Flexural Modulus 2,200 – 2,500 MPa 2,000 – 2,300 MPa 2,300 – 2,600 MPa 4,500 – 5,500 MPa
Notched Impact Strength 45 – 55 kJ/m² 40 – 50 kJ/m² 25 – 35 kJ/m² 15 – 25 kJ/m²
HDT @1.8 MPa 105 – 115 °C 100 – 110 °C 95 – 105 °C 115 – 125 °C
Melt Flow Rate (240°C/5kg) 15 – 25 g/10min 30 – 50 g/10min 10 – 20 g/10min 10 – 18 g/10min
Flame Rating (UL94) HB HB V-0 HB
Key Profile Balanced all-rounder Easy flow for complex parts Safety compliance High stiffness

PC/ABS Reinforced (GF20) Key Advantages

✅ Significantly Enhanced Stiffness & Strength: Glass fiber reinforcement multiplies flexural modulus and tensile strength, enabling parts to bear greater loads without deformation.
✅ High Dimensional Stability & Low Warpage: Very low and isotropic shrinkage ensures parts maintain precise dimensions after molding and during service, ideal for structural assemblies.
✅ Greatly Improved Heat Resistance & Creep Resistance: HDT is significantly increased, and resistance to long-term deformation under load is far superior to unreinforced material.

Industry Applications:

the crucial role of injection molding in automotive industry

Explore the PC/ABS Alloy Series in Detail

Click on the links below to view comprehensive technical data, key advantages, and application details for each specific grade.

Grade Best For Overview Full Details
PC/ABS General Purpose Applications demanding an optimal balance of impact strength, heat resistance, and processability. The benchmark alloy grade, offering the classic combination of PC’s toughness and ABS’s ease of processing for a wide range of structural parts. View PC/ABS GP Full Data Sheet →
PC/ABS High Flow Thin-walled, complex geometry parts requiring excellent filling and surface finish. Engineered with enhanced melt flow, facilitating the molding of intricate designs and reducing cycle times without sacrificing key mechanical properties. View PC/ABS HF Full Data Sheet →
PC/ABS Flame Retardant (V-0) Electronic enclosures and components with mandatory fire safety requirements. A UL94 V-0 rated grade that combines inherent flame retardancy with good impact strength and thermal stability for safe electronic applications. View PC/ABS FR Full Data Sheet →
PC/ABS Reinforced (GF20) Structural components requiring higher stiffness, dimensional stability, and heat deflection temperature. Glass fiber reinforced grade that significantly boosts rigidity and creep resistance while maintaining good overall toughness. View PC/ABS GF20 Full Data Sheet →

Powering Innovation Across Industries (PC/ABS Series)

Industry Key Applications
Automotive Interior trim (instrument panels, pillar covers, glove box doors), exterior components (wheel covers, mirror housings), and connectors requiring heat resistance & aesthetics. Explore Automotive Solutions →
Electrical & Electronics Durable housings for laptops, monitors, printers, power tools, and consumer electronics that demand a balance of impact strength, heat resistance, and good surface finish. Discover E&E Solutions →
Consumer Appliances & Tools Vacuum cleaner bodies, blender and coffee maker housings, power tool grips, and other appliance components needing structural integrity and a premium feel. Explore Consumer Applications →
Industrial & Business Equipment Robust casings for printers, copiers, industrial control panels, and handheld scanners where durability and dimensional stability are critical. See Industrial Uses →
Medical & Specialty Devices Housings for non-implantable medical devices, diagnostic equipment, and specialty enclosures requiring a combination of cleanliness, durability, and compliance. Inquire About Specialty Uses → or  Contact for Special Uses →

Various application scenarios of PA plastics

 How to Choose the Right PC/ABS Grade?

In simple terms:
For most structural applications requiring the best all-around balance of toughness, heat resistance, and cost-effectiveness, choose PC/ABS General Purpose.
For complex, thin-walled designs such as intricate housings or large panels, select PC/ABS High Flow to ensure complete filling and a superior surface.
For safety-critical electrical/electronic parts that must meet flame retardancy standards, specify PC/ABS Flame Retardant (V-0).
For applications where maximum stiffness, minimal deflection, and higher thermal performance are critical, opt for PC/ABS Reinforced (GF20).
Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation.

Why Choose Us?

万翰详情 03

万翰详情 04

PC/ABS Reinforced (GF20) FAQ
Q1: How does impact strength change with glass fiber reinforcement?
Reinforcement increases stiffness but typically reduces notched impact strength, making the material more brittle. Failure mode shifts from ductile to more brittle. However, unnotched impact strength may remain or improve slightly. Avoid sharp notches and stress concentrators in part design.

Q2: What is the surface appearance of glass-reinforced PC/ABS?
Due to fiber exposure, parts exhibit a prominent fiber pattern (“fiber readout”), reduced gloss, and a matte texture. This is considered an “engineering surface.” Painting is required for a high-gloss finish. Mold texturing can effectively mask the fiber pattern.

Q3: Are there special equipment requirements for processing GF20?
Yes, two main points: Wear-Resistant Equipment: Glass fibers are abrasive. Use bimetallic screws/barrels and hardened mold steels (e.g., H13). Mold Design: Gates and runners should be slightly enlarged to reduce shear and wear; venting needs to be more generous.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.

Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information