PEEK vs PEI — High-Temperature Engineering Plastics Compared

PEEK vs PEI illustration 1

High-Temperature Performance

PEEK and PEI (Ultem) are leading high-temperature engineering plastics.

Key Differences

Property PEEK PEI
Continuous Use Temp 250°C 170°C
Chemical Resistance Excellent Good
Cost $150-300/kg $30-60/kg

Frequently Asked Questions

Is PEEK stronger than PEI?

At room temperature, PEI has higher tensile strength. However, PEEK maintains properties better at elevated temperatures.

Where can I source PEEK and PEI?

Nylonplastic supplies both materials in rod, sheet, and tube forms.

PEEK vs PEI — Frequently Asked Questions

Is PEEK stronger than PEI?

At room temperature, PEI has higher tensile strength. PEEK maintains properties better at elevated temperatures.

Where can I source PEEK and PEI materials?

Nylonplastic supplies both materials in rod, sheet, and tube forms.