Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics

Nylon is a practical engineering topic when you need to compare options, check limits, and choose a process with less risk.

Nylon vs POM Acetal comparison
Nylon and POM are both engineering plastics but serve different purposes

Nylon and POM (polyoxymethylene, also known as acetal or Delrin) are two of the most important engineering plastics. Both are widely used for precision mechanical components, but their distinctly different properties make each better suited for specific applications.

Mechanical Properties Head-to-Head

Property PA6 (Nylon) POM (Acetal)
Tensile Strength (MPa) 70-85 60-70
Flexural Modulus (GPa) 2.5-3.0 2.6-2.9
Elongation at Break (%) 50-150 25-75
Density (g/cm³) 1.14 1.41
Mechanical properties radar chart
Nylon leads in strength and toughness; POM excels in dimensional stability

Wear and Friction: A Critical Difference

POM’s key advantage over nylon is its excellent wear resistance and low coefficient of friction (0.2-0.35 against steel), making it preferred for gears, bearings, and sliding components.

Moisture Absorption

Moisture absorption comparison
POM absorbs virtually no water, while nylon shows significant moisture uptake

POM absorbs less than 0.3% water even at saturation, while nylon absorbs 2.5-9.5% depending on conditions. This means POM parts maintain consistent dimensions regardless of humidity.

Chemical Resistance

Nylon is resistant to oils, greases, fuels, and alkalis. POM offers excellent resistance to organic solvents, oils, and neutral chemicals but is attacked by strong acids.

Thermal Properties

Property PA6 POM
Melting Point (°C) 220 165-175
HDT at 1.8 MPa (°C) 65 95-110
Continuous Use Temp (°C) 80-100 90-100
Thermal properties comparison
POM maintains stiffness better at elevated temperatures

Application Guide

Choose Nylon When:

  • Impact resistance and toughness are critical
  • Parts experience dynamic loading
  • Higher temperature resistance is needed (PA66)

Choose POM When:

  • Dimensional stability in varying humidity is critical
  • Low friction and wear resistance are priorities
  • Parts operate in wet environments
  • Precision mechanical components are needed

Our Capabilities

With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We machine both nylon and POM for precision applications. Get a quote within 24 hours.

FAQ

When is Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics a good option?

Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

Check part size, material properties, surface finish, dimensional tolerance, heat exposure, load direction, and whether post-processing is required.

How does Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics compare with CNC machining?

3D printing can create complex shapes quickly, while CNC machining is often stronger for precise surfaces, tighter tolerances, and production-grade materials.

What affects the cost of Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

Cost depends on material, build volume, print time, layer height, support removal, finishing, inspection, and the number of parts in the build.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.

Related Reading

Scroll to Top