Chemical Structure Differences

The fundamental difference between PA6 (Nylon 6) and PA66 (Nylon 66) lies in their molecular structure:

  • Nylon 6: Made from caprolactam, has 6 carbon atoms in each repeating unit. Less crystalline structure.
  • Nylon 66: Made from hexamethylenediamine and adipic acid, has two 6-carbon chains. More crystalline structure.

Mechanical Properties Comparison

PropertyPA6PA66
Tensile Strength70-85 MPa80-100 MPa
Flexural Modulus2.5-3.0 GPa2.8-3.5 GPa
Elongation at Break30-100%15-60%
Notched Izod Impact50-100 J/m40-80 J/m
Melting Point220°C260°C
HDT at 1.8 MPa70°C90°C

Moisture Absorption

Moisture absorption is critical for nylon applications:

ConditionPA6PA66
At 50% RH2.5-3.0%2.0-2.5%
Saturation8-10%6-8%

Processing Characteristics

Nylon 6 Processing

  • Melting Point: 220°C
  • Processing Range: 240-280°C
  • Mold Temperature: 40-80°C

Nylon 66 Processing

  • Melting Point: 260°C
  • Processing Range: 280-320°C
  • Mold Temperature: 60-90°C

Applications by Material

Nylon 6 Applications

  • Gears and sprockets
  • Industrial monofilament
  • Film and packaging
  • Consumer products

Nylon 66 Applications

  • Automotive under-hood components
  • Electrical connectors
  • High-temperature bearings
  • Precision mechanical components

Reinforced Grades

Both materials are commonly reinforced with glass fiber:

GradePA6 + GF30PA66 + GF30
Tensile Strength140-160 MPa170-200 MPa
HDT (1.8 MPa)205°C+250°C+
Moisture Absorption1.0-1.5%0.8-1.2%

Selection Summary

Choose Nylon 6 when:

  • Impact resistance is critical
  • Cost sensitivity is high
  • Operating temperatures are moderate

Choose Nylon 66 when:

  • Higher mechanical strength is required
  • Elevated temperatures are expected
  • Dimensional stability is critical

Frequently Asked Questions

Is Nylon 66 stronger than Nylon 6?

Yes. Nylon 66 typically offers 15-25% higher tensile strength due to more crystalline structure.

Which nylon is better for gears?

Both work well. PA6 is preferred for impact-loaded gears due to higher toughness. PA66 is better for high-load, high-temperature gear applications.

Where can I source quality PA6 and PA66?

Nylonplastic supplies both grades in natural, colored, and reinforced versions. Contact us for samples.

Nylon 6 vs Nylon 66 — Frequently Asked Questions

Is Nylon 66 stronger than Nylon 6?

Yes. Nylon 66 typically offers 15-25% higher tensile strength (80-100 MPa vs 70-85 MPa) due to more crystalline structure.

Which nylon is better for gears?

Both work well. PA6 is preferred for impact-loaded gears due to higher toughness. PA66 is better for high-load, high-temperature applications.

Where can I source quality PA6 and PA66 granules?

Nylonplastic supplies both grades in natural, colored, and reinforced versions. Contact us for samples.

Let's Craft Your Custom Solution

This field is required.
This field is required.
This field is required.
This field is required.

Which absorbs less moisture?

PA66 absorbs ~1.5% moisture at equilibrium vs PA6 at ~2.5%. This affects dimensional stability and mechanical properties.

Which is easier to machine?

PA6 machines more predictably with less burring. PA66 higher hardness requires sharper tooling but produces cleaner edges.