PA6 GF25 Material Overview
PA6 GF25 is a 25% glass-fiber-reinforced nylon 6 compound supplied as pellets. The reference grade is PA6 WHG25A. Evaluate it for reinforced housings, brackets and fan structures using the part drawing, service conditions and agreed sample checks.
| Item | Details |
|---|---|
| Reference grade | PA6 WHG25A |
| Polymer | PA6 (nylon 6) |
| Reinforcement | 25% glass fiber |
| Form | Pellets for material-supply inquiries |
| Color and processing | Confirm the offered grade and current processing guidance |
Reference Material Properties
Typical values for PA6 WHG25A from the linked supplier PDF.
| Property | Typical value | Test method |
|---|---|---|
| Tensile strength | 124 MPa | ISO 527-2 |
| Tensile strain at break | 10% | ISO 527-2 |
| Flexural modulus | 5300 MPa | ISO 178 |
| Deflection temperature under load | 175 °C | ISO 75-2/B |
| Density | 1.31 g/cm³ | ISO 1183 |
Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Only rows with a usable property, unit and method are reproduced; request clarification of the remaining sheet entries before relying on them for design.
Application Review

Reinforced housings
Check fastener locations, wall transitions and assembly loads. Review weld-line positions and moisture-conditioned dimensions during trials.
Mounting brackets
Define bolt loads, insert retention and the critical reference faces. Check long-term deflection under the expected temperature and moisture exposure.
Fan structures
Review blade or frame geometry, balance and attachment points. Validate vibration, clearance and the actual duty cycle on molded components.
Processing and Part Checks
Use WHG25A-specific processing guidance. Plan gates and weld lines around loaded regions, account for fiber orientation and agree dimensional inspection conditions. Keep the general GF25 material distinct from flame-retardant variants.
For component production, review our injection molding service. For other resin options, browse engineering plastic materials.
Material Supply and Manufacturing Support
Nylon Plastic connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.



Grade and formulation selection
Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.
Quality documents for your order
Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.
Support beyond resin pellets
For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.
Cooperating Factory Management-System Certificates
The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.
Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.
Frequently Asked Questions
What material does this page cover?
PA6 GF25 is a 25% glass-fiber-reinforced nylon 6 compound supplied as pellets. The reference grade is PA6 WHG25A. Evaluate it for reinforced housings, brackets and fan structures using the part drawing, service conditions and agreed sample checks.
Is this the same material as PA6 GF25 FR?
No. This page covers the general glass-filled WHG25A reference. The PDF does not establish a flame-retardant classification. Specify the exact formulation and test requirements if flame performance is needed.
Are these values a production specification?
No. They are typical reference values for PA6 WHG25A. Agree the current grade, test conditions, acceptance limits and required documents for the order.
Do the images show the exact supplied color and finished parts?
The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.
What is required for a material replacement?
Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.
What should I send for a quote or sample request?
Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.
Related Material Grades
Request Material Data and a Quote
Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.