PA6 GF35 Glass Fiber Reinforced Nylon 6 Pellets

PA6 GF35 is nylon 6 reinforced with 35% glass fiber, supplied as pellets for injection molding. It is used for reinforced housings, brackets and structural parts where stiffness and dimensional control matter.

Material: 35% glass-fiber-reinforced nylon 6, in pellet form.

Reference grade: PA6 WHG35A; typical tensile strength 175 MPa and flexural modulus 7000 MPa.

Applications: Power-tool frames, automotive brackets, industrial housings and impellers.

Selection: Share the part, operating conditions, color and material quantity.

Categories: ,

PA6 GF35 Material Overview

PA6 GF35 is nylon 6 reinforced with 35% glass fiber, supplied as pellets for injection molding. It is used for reinforced housings, brackets and structural parts where stiffness and dimensional control matter.

Item Details
Polymer PA6 (nylon 6)
Reinforcement 35% glass fiber
Form Pellets
Reference grade PA6 WHG35A
Processing Injection molding

Typical Material Properties

Reference grade: PA6 WHG35A. The following values are from the supplier datasheet linked below; they are typical material values, not finished-part specifications.

Property Typical value Unit Test method
Tensile strength 175 MPa ISO 527-2
Tensile strain at break 9 % ISO 527-2
Flexural modulus 7000 MPa ISO 178
HDT, method B 175 °C ISO 75-2/B
Density 1.40 g/cm³ ISO 1183
Molding shrinkage 0.5 % ISO 2577

HDT is reported under method B. The source does not state specimen conditioning. Confirm the current grade and test conditions before design approval.

Download PA6 WHG35A supplier datasheet (PDF)

PA6 GF35 Applications

Nine illustrative PA6 GF35 application and development examples; see the descriptions below
Illustrative applications; confirm the selected grade for your part. Tap the image to enlarge.

Power-tool gearbox housings and load-bearing frames.

Reinforced shells and frames support gears, bearings and fasteners. Check screw bosses, weld lines and vibration loads in the molded part.

Automotive brackets and industrial housings.

Mounting brackets, covers and machinery housings need repeatable fit around inserts, ribs and attachment points. Review the load direction and moisture exposure when setting tolerances.

Fan impellers, pump components and appliance frames.

These parts combine rotating or assembly loads with temperature exposure. Confirm fluid compatibility and validate the molded component for its duty cycle.

Processing and Part Checks

Use the selected grade’s drying and molding instructions. Check gate position, fiber orientation, weld lines, shrinkage and critical dimensions during trials. Confirm performance on parts made with the intended tool and process.

For finished components, continue to injection molding. For a material comparison, use the engineering plastics range.

Material Supply and Manufacturing Support

Nylon Plastic connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

PA6 GF35 — Frequently Asked Questions

What is PA6 GF35?

PA6 GF35 is nylon 6 reinforced with 35% glass fiber, supplied as pellets for injection molding. The PA6 WHG35A datasheet on this page is the supplier reference for the listed typical properties.

Which parts can use PA6 GF35?

Typical candidates include power-tool gearbox housings, automotive mounting brackets, machinery covers, fan impellers and appliance frames. Ribs, screw bosses, load direction and weld lines need checking in the molded part.

Can I use these datasheet values as finished-part specifications?

No. They are typical values for PA6 WHG35A test specimens. The source does not state specimen conditioning; agree the conditioning, test method and acceptance criteria for your part before approval.

What should be checked before molding PA6 GF35?

Follow the selected grade’s drying instructions. Review moisture exposure, gate position, fiber orientation and shrinkage before setting critical dimensions. Confirm fit and performance with the intended tool and process.

Is this PA6 GF35 grade flame retardant?

A glass-fiber percentage does not establish a flame rating. If your part requires a flame classification, send the standard and specimen thickness so the matching formulation and supporting record can be checked.

What do you need to quote PA6 GF35?

Send the application, current grade or material target, color, quantity, service conditions and delivery destination. For molded parts, add the drawing, critical dimensions and expected production quantity.

Request Material Data and a Quote

Send the application, current material if available, service temperature, load or fluid exposure, color, expected quantity and delivery destination. Add a drawing when finished parts are needed.

Request PA6 GF35 TDS and Quote