PA6 GF60 Technical Specifications (Estimated)
| Property | Value | Test Standard |
|---|---|---|
| Glass Fiber Content | 60% (±2%) | ISO 1172 |
| Tensile Strength | 170 – 230 MPa | ISO 527 |
| Flexural Modulus | 10,000 – 16,000 MPa | ISO 178 |
| Impact Strength (Notched Izod) | 7 – 10 kJ/m² | ISO 180 |
| Heat Deflection Temperature (HDT) | 205 – 225 °C @ 1.8 MPa | ISO 75 |
| Melting Point | 215 – 230 °C | ISO 3146 |
| Moisture Absorption (Equilibrium, 23°C/50% RH) | ~1.1% | ISO 62 |
PA6 Series Material Performance Comparison Table:
| Property | PA6 GF15 | PA6 GF30 | PA6 GF40 | PA6 GF50 | PA6 GF60 |
|---|---|---|---|---|---|
| Glass Fiber Content | 15% | 30% | 40% | 50% | 60% |
| Density (g/cm³) | 1.21 | 1.38 | 1.46 | 1.56 | 1.67 |
| Tensile Strength (MPa) | 118 | 165 | 185 | 200 | 220 |
| Elongation at Break (%) | 3.3 | 3.0 | 2.8 | 2.0 | 2.0 |
| Notched Impact Strength (kJ/m²) | 10 | 12 | 13 | 14 | 14 |
| Heat Deflection Temperature (℃, 1.8MPa) | 160 | 175 | 215 | 216 | 220 |
Key Advantages of PA6 G60:
Ultimate Stiffness and Load-Bearing Capacity
PA6 GF60 provides the highest possible flexural modulus and tensile strength in the standard PA6 GF series, offering metal-like rigidity that is ideal for structural components requiring absolute resistance to bending or deformation under extreme loads.
Exceptional Thermal and Dimensional Stability
With minimal moisture absorption and the highest HDT in its class, PA6 GF60 maintains unparalleled dimensional stability and mechanical properties in hot, humid, or thermally cycling environments, ensuring long-term precision.
Specialized Performance for Demanding Applications
Engineered for scenarios where conventional engineering plastics reach their limits, it delivers a unique combination of ultra-high strength, wear resistance, and thermal capabilities that can enable innovative, lightweight designs in advanced fields.
Enhanced Wear and Chemical Resistance
In addition to the good chemical resistance inherited from PA6, the high fiber load significantly improves wear resistance and reduces creep under sustained load, making it ideal for high-stress mechanical, automotive, and industrial applications.
Industry Applications:

PA6GF60 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.
Powering Innovation Across Industries
| Industry | Key Applications |
|---|---|
| Automotive | Engine covers, intake manifolds, structural brackets, sensor housings, connectors. Explore Automotive Applications → |
| Electrical & Electronics | Circuit breakers, switches, connector housings, insulating components. Discover E&E Solutions → |
| Industrial Equipment | Gears, bearings, machine housings, rollers, mechanical components. See Industrial Uses → |

How to Choose?
In simple terms:
-
For good toughness or cost-effectiveness, consider PA6 GF15.
-
For balanced overall performance, choose PA6 GF30.
-
For higher stiffness, strength, and heat resistance, and where cost is less sensitive, consider PA6 GF40/50/60. Generally, higher glass fiber content improves these properties.
Why Choose Us?


FAQ Section:
Q: Can I get a sample before placing an order?
A: Yes! We provide free samples for qualified projects.
Q: What’s the lead time for production?
A: Standard grades: 5-7 days; Custom formulations: 2-3 weeks.
Q: Do you provide material certifications?
A: Yes, we provide full material documentation and certifications.