PPS Engineering Plastics — A Comprehensive Guide to Polyphenylene Sulfide

PPS polyphenylene sulfide high-temperature engineering plastic - Nylonplastic

What Is PPS?

Polyphenylene Sulfide (PPS) is a high-performance engineering thermoplastic known for outstanding chemical resistance and thermal stability.

Key Properties

  • Continuous Service Temp: 200–220°C
  • Melting Point: 280°C
  • Chemical Resistance: Exceptional — resists acids, bases, solvents
  • UL94 Rating: V-0
  • Hydrolysis: Excellent resistance

Applications

PPS is used in automotive under-hood components, industrial pump parts, electrical connectors, and medical devices requiring sterilizability.

Grades Available

  • Unfilled: Maximum toughness
  • GF30/40%: Glass fiber reinforced for stiffness
  • CF10/30%: Carbon fiber for wear resistance
  • PTFE-filled: Self-lubricating grades

Sourcing PPS from China

Nylonplastic supplies PPS compounds with full technical documentation and export support.

Let's Craft Your Custom Solution

This field is required.
This field is required.
This field is required.
This field is required.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top