Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide

nylon 6 plastic pellets granules industrial packaging
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide
Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide

Chemical Structure Differences

The fundamental difference between PA6 (Nylon 6) and PA66 (Nylon 66) lies in their molecular structure:

  • Nylon 6: Made from caprolactam, has 6 carbon atoms in each repeating unit. Less crystalline structure.
  • Nylon 66: Made from hexamethylenediamine and adipic acid, has two 6-carbon chains. More crystalline structure.

Mechanical Properties Comparison

Property PA6 PA66
Tensile Strength 70-85 MPa 80-100 MPa
Flexural Modulus 2.5-3.0 GPa 2.8-3.5 GPa
Elongation at Break 30-100% 15-60%
Notched Izod Impact 50-100 J/m 40-80 J/m
Melting Point 220°C 260°C
HDT at 1.8 MPa 70°C 90°C

Moisture Absorption

Moisture absorption is critical for nylon applications:

Condition PA6 PA66
At 50% RH 2.5-3.0% 2.0-2.5%
Saturation 8-10% 6-8%

Processing Characteristics

Nylon 6 Processing

  • Melting Point: 220°C
  • Processing Range: 240-280°C
  • Mold Temperature: 40-80°C

Nylon 66 Processing

  • Melting Point: 260°C
  • Processing Range: 280-320°C
  • Mold Temperature: 60-90°C

Applications by Material

Nylon 6 Applications

  • Gears and sprockets
  • Industrial monofilament
  • Film and packaging
  • Consumer products

Nylon 66 Applications

  • Automotive under-hood components
  • Electrical connectors
  • High-temperature bearings
  • Precision mechanical components

Reinforced Grades

Both materials are commonly reinforced with glass fiber:

Grade PA6 + GF30 PA66 + GF30
Tensile Strength 140-160 MPa 170-200 MPa
HDT (1.8 MPa) 205°C+ 250°C+
Moisture Absorption 1.0-1.5% 0.8-1.2%

Selection Summary

Choose Nylon 6 when:

  • Impact resistance is critical
  • Cost sensitivity is high
  • Operating temperatures are moderate

Choose Nylon 66 when:

  • Higher mechanical strength is required
  • Elevated temperatures are expected
  • Dimensional stability is critical

FAQ

When is Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide a good option?

Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide?

Check part size, material properties, surface finish, dimensional tolerance, heat exposure, load direction, and whether post-processing is required.

How does Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide compare with CNC machining?

3D printing can create complex shapes quickly, while CNC machining is often stronger for precise surfaces, tighter tolerances, and production-grade materials.

What affects the cost of Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide?

Cost depends on material, build volume, print time, layer height, support removal, finishing, inspection, and the number of parts in the build.

Let's Craft Your Custom Solution

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.

Related Reading

Scroll to Top