Nylon Material Certifications: FDA, EU, NSF, and ISO Standards

Complete guide to nylon material certifications for food, medical, water, and industrial applications — FDA, EU Regulation 10/2011, NSF, WRAS, and ISO standards.

Material Certifications

Why Material Certifications Matter in Nylon Sourcing

Material Certifications

For engineers and procurement managers specifying nylon materials, certifications are not bureaucratic formalities — they are the legal and technical foundation that determines where your parts can be used. A nylon part that meets all mechanical requirements but lacks food-contact certification cannot legally be used in food processing equipment in the EU or US. Medical device applications require FDA device master file compatibility and ISO 10993 biocompatibility testing.

This guide provides a comprehensive overview of the certifications most relevant to nylon material selection, with practical guidance on what each means for your application.

US FDA Food Contact Regulations

The US FDA regulates food contact materials under 21 CFR (Code of Federal Regulations) Parts 174-180. For nylon, the key regulation is 21 CFR §177.1500, which establishes the conditions for safe use of nylon resins in food contact:

21 CFR §177.1500 — Nylon Resins:
This regulation specifies:
– Permitted nylon types (PA6, PA66, PA6/66 copolymer, PA11, PA12)
– Maximum residual monomer content
– Extraction limits (specific solvents and conditions)
– Temperature limitations for different food types

Key Limitations:

Fatty foods Up to 250°F (121°C) With extraction limitations
Dry foods Room temperature only No temperature restriction

What FDA compliance means in practice:
– The nylon resin is FDA-compliant (21 CFR §177.1500 listed)
– Colorants and additives used must also be FDA-approved for food contact
– The part manufacturer must ensure processing conditions don’t introduce contaminants
– FDA compliance is a starting point — specific applications may require additional testing

Not all FDA-listed nylons are equivalent — KSAN (Korea), BASF (Ultramid), DuPont (Zytel), and DSM (Stanyl) all have FDA-listed nylon grades, but they differ in additives, processing, and extraction profiles. Always request the FDA Letters of No Objection (LONO) or Food Contact Substance Notifications (FCN) from your material supplier.

EU Regulation 10/2011 for Food Contact Plastics

The EU has the most comprehensive food contact regulation for plastics. EU Regulation 10/2011 (and its amendments) establishes:

Dual Listing System:
The regulation lists:
1. Authorized monomers and starting substances (Annex I) — the chemical building blocks
2. Authorized additives (Annex II) — colorants, stabilizers, plasticizers
3. Specific Migration Limits (SMLs) — maximum allowed migration of each substance into food
4. Overall Migration Limit (OML) — 60 mg/kg food for total migrants

Nylon-Specific Requirements:
Nylon monomers (caprolactam for PA6, adipic acid and hexamethylenediamine for PA66) are specifically listed in Annex I. However, the additives used — catalysts, antioxidants, slip agents — must individually appear in the authorized list.

Key Compliance Points:

Specific Migration of caprolactam 15 mg/kg food
Primary aromatic amines (PAAs) ND (not detectable, 0.01 mg/kg)

Important: EU Regulation 10/2011 requires documentation of compliance including:
– Declaration of Compliance (DoC) from the material manufacturer
– Supporting technical documentation
– Batch traceability

For imported materials, request the EU 10/2011 compliance statement with specific SML test data from an accredited laboratory.

Medical Device Applications: FDA and ISO 10993

Nylon used in medical devices requires FDA device registration and ISO 10993 biocompatibility testing:

FDA Medical Device Regulation:
– Class I devices: General controls, many exempt from 510(k)
– Class II devices: Require 510(k) premarket notification — must demonstrate substantial equivalence to predicate device
– Class III devices: Require PMA (premarket approval) — most rigorous review

For material suppliers, FDA Device Master File (MAF) registration allows proprietary data sharing with device manufacturers without revealing trade secrets.

ISO 10993 Biocompatibility Testing:
This series of standards tests material biological safety. Key tests for nylon:

Test Standard What It Evaluates
Cytotoxicity ISO 10993-5 Cell death/viability in cell culture
Sensitization ISO 10993-10 Allergic reaction potential
Irritation ISO 10993-10 Skin/eye/mucosal irritation
Acute Systemic Toxicity ISO 10993-11 Toxic response to extracts
Implantation ISO 10993-6 Tissue response to implanted material

USP Class VI:
For pharmaceutical and medical device applications, USP Class VI testing is often required in addition to ISO 10993. This three-tiered test (systemic injection, intracutaneous, implantation) evaluates acute systemic and local tissue response.

Nylon’s Biocompatibility Profile:
PA6 and PA66 have a generally favorable biocompatibility profile — routinely passing ISO 10993-5 cytotoxicity and sensitization tests. However, residual monomers (caprolactam, hexamethylenediamine) can cause issues at high extraction levels. Medical-grade nylons have tighter monomer specifications.

Water and Plumbing Certifications

For nylon in potable water and plumbing applications, regional certifications are required:

NSF/ANSI 61 — Drinking Water System Components:
This North American standard establishes health effects criteria for devices and components that contact drinking water. NSF 61 covers:
– Extraction testing for regulated contaminants
– Maximum contaminant levels (lead, phthalates, BPA, etc.)
– Threshold of toxicological concern (TTC) approach for non-listed substances

Nylon compounds seeking NSF 61 certification must pass extraction testing at standardized conditions. Common grades: PA66-GF for hot water plumbing, PA12 for cold water and fuel lines.

WRAS (Water Regulations Advisory Scheme) — UK:
WRAS approval requires materials to not contaminate water or promote microbial growth. Testing includes:
– Non-toxicity to water organisms
– Taste and odor testing
– Extraction testing for regulated substances

KTW (Kunststoffe für Trinkwasser — Germany):
German drinking water certification with specific extraction limits for plasticizers, antioxidants, and colorants. More stringent than NSF 61 in some areas, particularly for plasticizer content.

ACS (Attestation de Conformité Sanitaire — France):
French sanitary certification based on AFNOR standards. Requires declaration of all components and extraction testing in French-accredited laboratories.

For international projects: Always verify the specific regional water certification required. Many countries have their own standards that may differ significantly.

UL Flammability and Electrical Certifications

For electrical and fire safety applications:

UL 94 Flammability Classification:
The most common flammability standard for plastics in electrical applications:

Rating Test Typical Nylon Grades
HB Horizontal burn, self-extinguishing Standard PA6, PA66
V-2 Vertical burn, 30s max after flame removal PA66 with flame retardant
V-1 Vertical burn, 30s max, no dripping FR modified PA66
V-0 Vertical burn, 10s max, no dripping FR PA66, FR PA6
5VB 5V test, no burn-through, panel Premium FR grades

Glow Wire Flammability Index (GWFI) and Glow Wire Ignition Temperature (GWIT):
More relevant for electrical components that may be heated by current:

Property Standard PA66 FR PA66
— — —
GWIT (775°C) Fails Passes at 0.8mm

RTI (Relative Thermal Index):
Underwriters Laboratories assigns RTI values indicating maximum continuous use temperature:

Property PA66 PA66-GF30 FR PA66
RTI Electrical 85°C 130°C 130°C
RTI Impact 75°C 130°C 130°C

CTI (Comparative Tracking Index):
Measures resistance to electrical tracking (surface leakage under voltage). PA66 typically achieves CTI 500-600V. FR grades often reduce CTI to 250-400V. For EV applications requiring CTI >600V, special high-CTI grades are needed.

FAQ

How do you know whether Nylon Material Certifications: FDA, EU, NSF, and ISO Standards fits a part?

Nylon Material Certifications: FDA, EU, NSF, and ISO Standards fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Nylon Material Certifications: FDA, EU, NSF, and ISO Standards?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for Nylon Material Certifications: FDA, EU, NSF, and ISO Standards?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should Nylon Material Certifications: FDA, EU, NSF, and ISO Standards be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.

Related Reading

Scroll to Top