PA11 GF10 with 10% Glass Fiber | Nylon Plastic

PA11 GF10 is an engineering thermoplastic composite based on bio-based Nylon 11 (PA11) reinforced with 10% glass fibers. This entry-level reinforced grade is designed to offer a straightforward and economical performance upgrade, enhancing the stiffness and heat resistance of parts that must also withstand demanding environmental and chemical exposure.

Why Choose Our PA11 GF10?
✅ Your Gateway to Reinforced Bio-Polymers: We deliver the most accessible entry point into glass-fiber reinforced PA11, helping you achieve better part performance without a significant cost leap.
✅ Master of Core Property Retention: Our PA11 GF10 is engineered to boost key properties like stiffness while safeguarding the unparalleled toughness and chemical resistance your application relies on.
✅ Simplified Transition to Advanced Materials: We provide the processing guidance and support to make your shift from standard to reinforced PA11 smooth and successful, minimizing production risks.
✅ Sustainable Solution for Demanding Basics: We partner with you to implement this material in fluid handling, automotive clips, and industrial components where durability and an eco-profile matter.

Categories: , Brand:

万翰详情 01

PA11 GF10 Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 10% ISO 1172
Tensile Strength 90 – 110 MPa ISO 527
Flexural Modulus 4,500 – 5,500 MPa ISO 178
Notched Impact Strength 12 – 16 kJ/m² ISO 180
HDT @1.8 MPa 155 – 165 °C ISO 75
Water Absorption (24h) ~0.8% ISO 62

PA11 GF Series Performance Comparison Table (Estimated Typical Values)

Property PA11 GF10 PA11 GF20 PA11 GF30 PA11 GF40 PA11 GF50
Glass Fiber Content 10% 20% 30% 40% 50%
Tensile Strength 90 – 110 MPa 115 – 135 MPa 135 – 155 MPa 150 – 170 MPa 165 – 185 MPa
Flexural Modulus 4,500 – 5,500 MPa 6,500 – 7,800 MPa 8,500 – 10,000 MPa 10,500 – 12,500 MPa 12,500 – 15,000 MPa
Notched Impact Strength 12 – 16 kJ/m² 10 – 14 kJ/m² 9 – 12 kJ/m² 8 – 11 kJ/m² 7 – 10 kJ/m²
HDT @1.8 MPa 155 – 165 °C 160 – 170 °C 165 – 175 °C 170 – 180 °C 175 – 185 °C
Water Absorption (24h) ~0.8% ~0.7% ~0.6% ~0.5% ~0.4%
Key Profile Stiffness upgrade Balanced performance Structural benchmark High rigidity Maximum performance

PA11 GF10 Key Advantages

✅ Cost-Effective Stiffness Enhancement: Offers a meaningful and affordable increase in rigidity and dimensional stability over unreinforced PA11, making it a practical first step into reinforced bio-plastics.
✅ Retained Exceptional Toughness & Chemical Resistance: Preserves the high impact strength and outstanding resistance to fuels, oils, and chemicals that are the hallmark of the PA11 matrix.
✅ Inherent Sustainability with Improved Performance: Provides a clear upgrade in mechanical performance while maintaining the bio-based origin and low moisture absorption benefits of PA11.

Industry Applications:

the crucial role of injection molding in automotive industry

Explore the PA11 Glass Fiber Series in Detail

Click on the links below to view comprehensive technical data, key advantages, and application details for each specific grade.

Grade Best For Overview Full Details
PA11 GF10 Cost-effective enhancement of stiffness & dimensional stability for durable, chemical-resistant parts. The most accessible reinforced grade, offering a clear boost in rigidity and heat resistance while retaining the excellent toughness and chemical resistance of PA11. View PA11 GF10 Full Data Sheet →
PA11 GF20 Technical components requiring a balanced upgrade in mechanicals, precision, and environmental resistance. A balanced performer, providing significantly higher stiffness and strength than GF10, ideal for more demanding structural applications in harsh conditions. View PA11 GF20 Full Data Sheet →
PA11 GF30 High-performance parts demanding toughness, rigidity, and stability in aggressive chemical or humid environments. The benchmark grade, delivering an optimal balance of high mechanical properties, thermal resistance, and PA11‘s signature durability. View PA11 GF30 Full Data Sheet →
PA11 GF40 Ultra-stiff components where minimal deflection and maximum dimensional precision are critical in demanding settings. Engineered for maximum rigidity and exceptional long-term dimensional stability from a bio-based foundation. View PA11 GF40 Full Data Sheet →
PA11 GF50 Maximum sustainable performance for structural metal replacement in chemically challenging applications. The pinnacle grade, offering the highest stiffness and strength in the series for the most advanced sustainable engineering designs. View PA11 GF50 Full Data Sheet →

Powering Innovation Across Industries (PA11 GF Series)

Industry Key Applications
Automotive Fuel line components, clips and connectors, structural under-hood brackets, sensor housings exposed to fluids. Explore Automotive Solutions →
Industrial Fluid Handling Pump housings, valve bodies, compressor parts, and components in chemical processing equipment requiring corrosion resistance. See Industrial Uses →
Consumer & Sports Goods High-performance sports equipment (ski bindings, cleats), power tool housings requiring durability, and premium appliance components. Explore Consumer Applications →
Electrical & Specialized Connectors and housings in harsh environments, cable management systems, and specialized industrial components. Inquire About Specialty Uses →

Various application scenarios of PA plastics

Various application scenarios of PA plastics

How to Choose the Right PA11 GF Grade?

In simple terms:

For a cost-effective step into reinforced bio-based plastics with improved stiffness and stability for fluid-handling parts, consider PA11 GF10.
For the optimal balance of enhanced mechanical properties, precision, and unmatched chemical/fuel resistance in demanding technical components, choose PA11 GF30. It is the performance benchmark for most structural uses in harsh environments.
For the ultimate stiffness and dimensional stability from a bio-based material in high-load, high-precision applications, consider PA11 GF50.
Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation.

Why Choose Us?

万翰详情 03

万翰详情 04

PA11 GF10 FAQ

Q1: What is the main benefit of PA11 GF10 over unreinforced PA11?
The primary benefit is a significant increase in flexural modulus (stiffness) and heat deflection temperature (HDT), allowing parts to carry more load and resist deformation better, especially in warmer environments. It also reduces molding shrinkage for improved dimensional accuracy.

Q2: Can PA11 GF10 be used for parts in constant contact with oil?
Yes, absolutely. PA11 GF10 inherits the excellent resistance to oils, greases, and hydraulic fluids from its PA11 base. This makes it suitable for components in machinery, automotive systems, or fluid transfer applications where both chemical resistance and some structural rigidity are needed.

Q3: How does processing PA11 GF10 differ from processing PA6 GF10?
Key differences include: Lower Processing Temperature: PA11 processes at 220-250°C vs. 280-310°C for PA6. Less Drying Criticality: While drying is still required, PA11 is less prone to hydrolysis than PA6. Different Mold Temperature: A mold temperature of 50-70°C is typical for PA11, potentially lower than for PA6.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information