Sink Marks in Injection Molding: DFM, Packing and Wall Thickness Guide

Sink marks in injection molding are shallow depressions on the part surface caused by uneven shrinkage, usually where thick walls, ribs, bosses, screw posts or heavy sections cool more slowly than surrounding material. Fixes usually require both DFM review and process tuning.

A molded part can pass basic dimensions and still fail visual inspection because of sink marks. For housings, covers, automotive trim and consumer-facing components, sink control should be planned before mold cutting through wall design, rib ratios, gate location and packing strategy.

Molded plastic housing with visible sink marks above bosses and ribs beside DFM samples and calipers

Common Causes of Sink Marks

Cause / material Typical sign or use Buyer or engineering action
Thick wall section Surface depression over heavy mass Core out thick areas and keep wall transitions gradual
Oversized ribs Sink opposite rib base Keep rib thickness lower than nominal wall
Heavy bosses Circular sink on visible surface Use support ribs and proper boss design
Gate freeze too early Poor packing in thick zones Review gate size, location and packing time
High shrinkage material More visible sink on PP, PE or crystalline resins Adjust DFM and shrinkage expectations by material

DFM Checks Before Tooling

  • Keep nominal wall thickness as uniform as practical.
  • Avoid abrupt transitions from thin walls to heavy sections.
  • Design ribs thinner than the main wall and add radius where needed.
  • Core out bosses instead of leaving solid plastic masses.
  • Place gates so thick zones can be packed before gate freeze.

Material Shrinkage and Sink Risk

Material / case Main concern Selection note
ABS Moderate sink risk Good for housings when ribs and bosses are designed correctly
PC / PC-ABS Moderate risk Cosmetic surfaces need stress and sink review
PP Higher shrinkage Control wall thickness and warpage together
POM Crystalline shrinkage Review precision features and packing
Glass-filled nylon Fiber orientation and differential shrinkage Check ribs, bosses and warpage

Buyer RFQ Details for Sink Mark Prevention

For a useful review, send the 3D model or 2D drawing, resin grade or target material, part photos if the defect already exists, machine and mold information if available, expected annual volume, cosmetic requirements, critical dimensions, application environment and any inspection standard. Nylon Plastic can review the design, material and molding route before tooling or production changes are made.

Sink Mark Diagnosis by Feature

Feature or Pattern Why It Sinks Design or Process Review
Sink over a rib Local mass cools later than the visible wall Reduce rib ratio, hollow the section, and confirm packing access
Sink around a boss Solid plastic around the post creates an uneven cooling section Use a cored boss, adequate draft, and a controlled wall transition
Sink near the flow end Pressure has decayed before the thick region is packed Review gate location, runner balance, hold pressure and freeze time
Sink changes after material substitution Shrinkage, viscosity, reinforcement and conditioning changed Recheck the exact grade, filler direction, drying and shrinkage assumptions

Higher packing pressure can hide a sink mark on one tool trial, but it may increase flash, stress, cycle time, or gate blush. A durable correction normally combines section design, gate access, cooling, material choice, and a validated packing window.

How Nylon Plastic Supports the Project

Nylon Plastic has supported material selection and finished plastic-part manufacturing since 2005. For sink mark prevention on molded plastic parts, the useful review connects the drawing, material, tooling or machining route, inspection state, and production plan before a quote is approved.

  • Review the visible surface, rib and boss geometry, material shrinkage, gate location, and expected conditioning state before tooling.
  • Compare unfilled PA with PA-GF20 or PA-CF30 only when the structural and dimensional requirements justify the change in flow and anisotropy.
  • Use sample parts, measured wall sections, cavity records, and defined cosmetic limits to close the DFM decision.

Related Reading

Sink marks surface depression on thick-walled injection molded parts with uniform wall design solution

Frequently Asked Questions

What causes sink marks in injection molding?

Sink marks usually come from uneven volumetric shrinkage in thick sections such as ribs, bosses, solid pads, or abrupt wall transitions. Packing, cooling, material, and gate access influence the result.

Can packing pressure remove sink marks?

It can reduce some sink marks when the gate remains open long enough, but excessive packing may create flash, stress, warpage, or a longer cycle. Correct the geometry and pressure window together.

Which materials are more sensitive to sink marks?

Every thermoplastic can show sink marks when section mass and cooling are poorly controlled. The exact grade, reinforcement, shrinkage, flow direction, and processing window should be checked rather than relying on a family label.

What should a sink mark DFM review include?

Provide the CAD model, wall and rib map, cosmetic zones, material or backup grade, gate concept, annual quantity, tolerance requirements, and photos or measurements of the defect.

Request a Sink Mark DFM Review

Send the part geometry, resin requirement, cosmetic zones, and target quantity for a design, tooling, and process review.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top